Corrosion and Stress Corrosion Testing of Aerospace Vehicle Structural Alloys: SpringerBriefs in Applied Sciences and Technology

Autor Russell Wanhill, Michael Windisch
en Limba Engleză Paperback – 4 iun 2018
This SpringerBrief discusses the determination and classification of the ambient temperature corrosion and stress corrosion properties of aerospace structural alloys, with emphasis on (1) aluminium alloys, modern (3rd generation) aluminium‒lithium alloys, stainless steels and titanium alloys and (2) some of the issues involved. Standard /reference data on environmental properties, including corrosion and stress corrosion, are mandatory for the qualification and certification of materials for aerospace vehicles, and also for the design of actual structures and components. Recommendations for further testing and evaluation are given at appropriate points in the text. The book concludes with a summary of the main topics.  
Citește tot Restrânge

Din seria SpringerBriefs in Applied Sciences and Technology

Preț: 40866 lei

Nou

Puncte Express: 613

Preț estimativ în valută:
7822 8499$ 6575£

Carte tipărită la comandă

Livrare economică 21 aprilie-05 mai

Preluare comenzi: 021 569.72.76

Specificații

ISBN-13: 9783319895291
ISBN-10: 331989529X
Pagini: 72
Ilustrații: XI, 63 p. 15 illus., 14 illus. in color.
Dimensiuni: 155 x 235 mm
Greutate: 0.12 kg
Ediția:1st ed. 2018
Editura: Springer International Publishing
Colecția Springer
Seria SpringerBriefs in Applied Sciences and Technology

Locul publicării:Cham, Switzerland

Cuprins

1. Introduction.- 2. Corrosion.- 3. Stress Corrosion Cracking (SCC).- 4. Environmental severities: natural/outdoor versus accelerated testing.- 5. Aluminium-lithium alloys: some corrosion and SCC issues.- 6. Stainless steels: some corrosion and SCC issues.- 7. Titanium alloys: special issues and aspects concerned with SCC testing.- 8. Summary.- Acknowledgements.- References.

Textul de pe ultima copertă

This SpringerBrief discusses the determination and classification of the ambient temperature corrosion and stress corrosion properties of aerospace structural alloys, with emphasis on (1) aluminium alloys, modern (3rd generation) aluminium‒lithium alloys, stainless steels and titanium alloys and (2) some of the issues involved. Standard /reference data on environmental properties, including corrosion and stress corrosion, are mandatory for the qualification and certification of materials for aerospace vehicles, and also for the design of actual structures and components. Recommendations for further testing and evaluation are given at appropriate points in the text. The book concludes with a summary of the main topics.  

Caracteristici

Initiates a new topic Provides a unique, independent and authoritative overview of the problem Treats a problem that is of major significance for aerospace (space) vehicle structures